Natural Botanical Dye, Mordant WOF% & Shibori Ratio Calculator

Weigh dry fabric or yarn once and get exact gram recipes for scouring, tannin pre-mordant, Potassium Alum or Aluminum Acetate, Cream of Tartar, dried dyestuff (Marigold, Madder, Cochineal, Indigo), Iron shift, plus Shibori resist fold visuals.

Quick Dye Vat Rule: Weigh textiles bone-dry first (WOF). Fill vat with enough water so goods swim freely (typically 15–20 L per kg), then dose mordants strictly by dry fiber percentage, not water volume.
GemsMakers Research Lab
| 📊 Open Datasets | ⚡ Free REST API | 🏷️ SVG Badges
1. Scour Agent + Pre-Tannin6g Soda Ash + 24g Gallnut
2. Primary Mordant Bath45g Alum + 18g Soda Ash
3. Botanical Dyestuff Weight150 g Dried Marigold
4. Iron Modifier + Dye Pot Size3.0 g Iron | Min 6 L Pot
Dry Weight of Fiber (WOF g)300 g
Fiber FamilyChemistry
Natural Dyestuff TargetShade Extract
Shade Depth / Saturation100% Standard
Iron Sadden Modifier (%)1.0% WOF
Iron Shift PreviewColor Tone

Companion Vat Helper: Multi-Garment Dry Weight Adder

Weighing several T-shirts, skeins, or napkins one by one on a kitchen scale? Add items here and sync total WOF grams straight into the recipe above.

Basket Items: 0 items (0 g total)

3-Step Lightfast Botanical Dye Workflow

1. Scour Thoroughly FirstEven "washed" fabric holds factory pectin, oils, and sizing. Simmer cotton with soda ash + pH-neutral detergent, or soak wool gently without agitation to stop felting.
2. Tannin -> Alum (Cellulose Two-Step)Cellulose grabs tannic acid before Potassium Alum + Soda Ash; never dump wool in high-alkaline soda ash or fibers dissolve and harshen.
3. Control Heat & Cure 48hKeep Madder under 70 C (160 F) so browns stay out of your reds, and allow dyed goods to dry and cure before washing out excess pigment.

Dye Chemistry Mistake Alert vs. Studio Master Fact

Mistake: Simmering Wool in Soda Ash & Boiling Madder

Boiling wool in alkaline soda ash breaks disulfide bonds and turns yarn brittle and felted, while boiling Madder root above 75 C pulls muddy brown tannins instead of true red alizarin.

Fact: Dedicated Acid/Alum vs. Cellulose Pots

Label dedicated stainless or enamel dye pots separately from food cookware, pre-wet all dry scoured fibers for 30 minutes before dipping, and dissolve alum completely in boiling water first.

60-Second Pre-Vat Dyeing Checklist

Standard Botanical Mordant & Scour Percentages (WOF%) Reference

Additive / ChemicalCellulose (Cotton/Linen)Protein (Wool/Silk)Key Purpose
Soda Ash (Sodium Carbonate)2% WOF scour (+12% Aluminum Acetate aid)NEVER on wool/silk (too alkaline!)Removes wax/pectin; sets Procion MX dyes
Oak Gallnut / Tara Tannin8–10% WOFOptional (0–3% WOF)Provides tannic anchor for cellulose alum bond
Potassium Alum (Alum Sulfate)15% WOF (2-bath w/ soda ash)10–15% WOFPrimary lightfast metallic mordant salt
Cream of TartarNot needed6% WOF (Wool brightener)Keeps wool soft and shifts cochineal warmer
Ferrous Sulfate (Iron)1–3% WOF post-bath0.5–1.5% WOF (5 min max)Shifts yellows to olive, pinks to plum/charcoal

Frequently Asked Questions

What does WOF (Weight of Fiber) mean in natural dyeing?

WOF stands for the completely dry weight of your fabric or yarn before wetting. Every scour agent, tannin, alum mordant, and dried botanical dye percentage is multiplied by dry fiber grams—not by the gallons of water in the pot.

Why do cotton and linen need tannin before alum while wool does not?

Cellulose fibers (cotton, linen, hemp) lack protein amino groups, so alum washes away easily unless anchored by tannic acid. Pre-treating with 8–10% WOF Oak Gallnut or Tara tannin binds alum permanently, whereas wool and silk bond directly to Potassium Alum + Cream of Tartar.

How much ferrous sulfate (iron) should I add to shift botanical colors?

Never exceed 1–2% WOF ferrous sulfate on wool or silk, or 3% WOF on cotton, and simmer briefly for 5–10 minutes max. Excess iron makes wool brittle and permanently weakens silk fibers.

What soda ash concentration works best for Procion MX cold-water tie-dye?

Mix roughly 15% WOF (or 1 US cup / ~240 g soda ash per gallon of warm soak water) and soak pre-scoured cotton garments for 15–20 minutes before ringing out and applying fiber-reactive dye.