Lead-Free Silver Electronics Solder (SAC305) Scrap Value & Joint Cost Calculator
Split Sn96.5/Ag3.0/Cu0.5 (SAC305), SAC405, and audio silver solder spools or wave-solder dross into exact pure silver vs. tin mass, intrinsic dollar share, and metal cost per 1,000 joints.
Even though SAC305 contains only 3.0% silver by weight, high silver spot makes that 3% silver worth more than the remaining 96.5% tin.
Quick Answer & Exact Silver Formula
A 1 lb (453.6 g) spool of SAC305 lead-free solder (96.5% Sn / 3.0% Ag / 0.5% Cu) contains 13.61 g (0.438 ozt) of pure silver and 437.7 g of tin. At $32.50/ozt silver and $31.00/kg tin, the intrinsic metal value totals $27.79 ($14.22 from silver and $13.57 from tin), costing $0.74 per 1,000 12 mg solder joints compared to $0.41 for low-silver SAC0307.
Silver Verification Checklist (0% Complete)
Verify solder alloy markings, tin-to-silver price ratios, and refinery settlement terms before pricing spools or wave-solder dross.
Common Silver-Bearing Electronics Solders: Composition, Melting Range & Value Drivers
Comparison of standard IPC lead-free SAC alloys, low-silver substitutes, audio eutectic wire, and legacy leaded silver solder per 1 kg.
| Alloy Designation | Composition (Sn / Ag / Cu / Pb) | Melting Range (C) | Ag Grams / 1 kg | Primary Electronics Application |
|---|---|---|---|---|
| SAC305 (IPC Standard) | 96.5% Sn / 3.0% Ag / 0.5% Cu | 217 - 220 C | 30.0 g (0.965 ozt) | Mainstream RoHS SMT reflow and wave soldering |
| SAC405 (High-Rel) | 95.5% Sn / 4.0% Ag / 0.5% Cu | 217 - 219 C | 40.0 g (1.286 ozt) | Aerospace, medical, and high-vibration BGA assemblies |
| SAC387 (Eutectic SAC) | 95.5% Sn / 3.8% Ag / 0.7% Cu | 217 C (Near-Eutectic) | 38.0 g (1.222 ozt) | Precision European SMT lines needing minimal pasty range |
| SAC0307 (Low-Ag) | 99.0% Sn / 0.3% Ag / 0.7% Cu | 217 - 227 C | 3.0 g (0.096 ozt) | Cost-sensitive consumer boards reducing silver BOM cost |
| Sn96.5 / Ag3.5 (96S) | 96.5% Sn / 3.5% Ag / 0% Cu | 221 C (Eutectic) | 35.0 g (1.125 ozt) | High-conductivity audio wiring, sensors, and step soldering |
| Sn96 / Ag4 (96/4) | 96.0% Sn / 4.0% Ag / 0% Cu | 221 - 229 C | 40.0 g (1.286 ozt) | Food-grade plumbing, stainless steel, and specialty joints |
| Sn62 / Pb36 / Ag2 | 62.0% Sn / 2.0% Ag / 36.0% Pb | 179 C (Eutectic) | 20.0 g (0.643 ozt) | Ceramic hybrid substrates and silver-metallized RF parts (non-RoHS) |
How It Works: 3-Step Silver Workflow
Select Solder Alloy & Mass
Pick SAC305, SAC405, Sn96.5/Ag3.5, Sn62/Pb36/Ag2, or Custom, then enter your spool, bar, or dross weight in grams, pounds, or kilograms.
Update Silver & Tin Spot Rates
Enter live silver spot per troy ounce and refined tin spot per kilogram in USD, EUR, or GBP, plus your average solder mass per PCB joint in milligrams.
Evaluate Value Share & Joint Economics
Inspect the SVG value-vs-mass bar to see how 3%-4% silver rivals 96% tin in dollar worth, and compare cost per 1,000 joints against SAC0307.
Silver Myth vs. Metallurgical Reality
SAC305 is only 3% silver, so the tin makes up 97% of the scrap value.
RealityTin trades around $28-$35 per kilogram whereas silver trades near $1,045 per kilogram ($32.50/ozt). Because silver is roughly 33 times more valuable per gram than tin, 3.0% silver routinely provides over half of SAC305's metal value.
Wave-solder dross sells for the exact same metal value as clean unused SAC305 bars.
RealityPot dross is a mix of metallic solder and tin-copper-silver oxides skimmed off the solder bath. Unless mechanically pressed or thermally recovered first, dross yields lower metallic recovery and faces refining treatment charges.
Lead-free SAC0307 and SAC305 can be tossed into the same scrap drum with Sn62/Pb36/Ag2.
RealityMixing even small amounts of 36%-lead Sn62/Pb36/Ag2 solder into RoHS lead-free tin-silver dross contaminates the melt for lead-free tin reclaimers and slashes payout rates.
Switching a PCB line from SAC305 to SAC0307 barely changes solder material spending.
RealityAt 12 mg per joint across 10 million joints per year (120 kg solder), dropping from 3.0% Ag to 0.3% Ag eliminates 3.24 kg (104 ozt) of silver annually, saving over $3,300 in pure metal cost alone.
Worked Real-World Silver Examples & Mistake-Avoidance
Example 1: 1 lb (453.6 g) SAC305 Electronics Spool
A standard 1 lb spool of 0.8 mm SAC305 rosin-core wire holds 13.61 g (0.438 ozt) of silver ($14.22 at $32.50/ozt) and 437.7 g of tin ($13.57 at $31.00/kg), giving $27.79 in pure element value despite retail wire spool markups.
Example 2: 5 kg SAC405 Wave-Solder Pot Cleanout
A 5 kg metallic ingot reclaimed from an aerospace SAC405 pot holds 200 g (6.43 ozt) of silver ($208.98) plus 4.775 kg of tin ($148.03), totaling $357.01 gross metal value before refiner assay and treatment fees.
Example 3: 1 Million PCB Solder Joints (SAC305 vs SAC0307)
At 12 mg per solder fillet, 1 million joints consume 12 kg of alloy. SAC305 carries $735 in intrinsic metal value ($0.74 per 1,000 joints) while SAC0307 drops intrinsic metal cost to $407 ($0.41 per 1,000 joints), saving $328 per million joints.
Frequently Asked Questions
How much pure silver is in a 1 lb spool of SAC305 solder?
A 1 lb (453.59 g) spool of SAC305 contains 3.0% silver by weight, which equals 13.61 grams or 0.4375 troy ounces of pure silver alongside 437.72 grams of tin and 2.27 grams of copper.
Why does silver account for half the value of SAC305 when it is only 3% of the weight?
Silver prices per gram (~$1.04/g at $32.50/ozt) are roughly 30 to 35 times higher than refined tin prices (~$0.031/g at $31/kg). Multiplying 3% weight by a 33x price premium makes the tiny silver fraction worth as much as the other 96.5% tin.
Can individuals profitably melt SAC305 solder wire to extract silver?
No. Hobby chemical or furnace separation of 3% silver from 96.5% tin is inefficient and generates heavy tin oxide sludge and metastannic acid waste. Commercial electronics solder reclaimers recover both tin and silver cleanly by vacuum distillation or electro-refining.
What is the difference between SAC305, SAC405, and SAC0307?
SAC305 (3.0% Ag) is the global electronics industry baseline balancing wetting and thermal fatigue resistance. SAC405 raises silver to 4.0% for extreme aerospace/automotive reliability, while SAC0307 trims silver to 0.3% to cut alloy cost on high-volume consumer boards.
How is solder pot dross priced by electronics recyclers?
Recyclers weigh the gross drum, melt a sample or run XRF/ICP assay on metallic beads vs oxide ash, and pay a percentage of both recoverable tin and silver minus a refining fee. High-metallic clean bars fetch 85%-94%, whereas powdery oxide dross yields less.
Does Sn62/Pb36/Ag2 audio or hybrid solder have higher or lower silver value than SAC305?
Sn62/Pb36/Ag2 contains 2.0% silver (one-third less silver than SAC305) and substitutes 36% lead for tin. Because lead is much cheaper than tin and silver is lower, its intrinsic scrap value per kilogram is substantially below SAC305.